Longitudinal thickness tensile strength | 800~1500(KN/m) | |||||||
Longitudinal elongation <=2% | <=2% | |||||||
Burner flame test | With cover: average<=3s, individual<=10s | |||||||
Without cover: average<=5s, individual<=15s | ||||||||
Surface resistant | <=3*108Ω | |||||||
Rubber thickness top (mm) | 1.5~8 | |||||||
Rubber thickness bottom(mm) | 1.5~4.5 |
We have a modern large R & D and quality inspection center, and the center has six rubber material laboratories, including material test, formula test, rubber mixing test and finished product test. 126 management and technical personnel are engaged in product research and development and quality inspection. From raw materials to finished products, each production step is tested with advanced test equipment, which ensures the reliable and stable product quality.
Longitudinal thickness tensile strength | 800~1500(KN/m) | |||||||
Longitudinal elongation <=2% | <=2% | |||||||
Burner flame test | With cover: average<=3s, individual<=10s | |||||||
Without cover: average<=5s, individual<=15s | ||||||||
Surface resistant | <=3*108Ω | |||||||
Rubber thickness top (mm) | 1.5~8 | |||||||
Rubber thickness bottom(mm) | 1.5~4.5 |
We have a modern large R & D and quality inspection center, and the center has six rubber material laboratories, including material test, formula test, rubber mixing test and finished product test. 126 management and technical personnel are engaged in product research and development and quality inspection. From raw materials to finished products, each production step is tested with advanced test equipment, which ensures the reliable and stable product quality.